Polydopamine-mediated modification of ZIF-8 onto magnetic nanoparticles for enhanced tetracycline adsorption from wastewater

Magnetic nanoparticle materials which could be used to remove tetracycline were confined seriously due to their poor stability and unsatisfactory reusability. Here, we facilely prepared novel zeolitic imidazolate framework-8 (ZIF-8) functionalized magnetic nanoparticles (Fe3O4@PDA-ZIF-8) adsorbent u...

Full description

Saved in:
Bibliographic Details
Published in:Chemosphere (Oxford) Vol. 308; p. 136249
Main Authors: Sheng, Daohu, Ying, Xintong, Li, Rui, Cheng, Siyao, Zhang, Cheng, Dong, Wei, Pan, Xihao
Format: Journal Article
Language:English
Published: Elsevier Ltd 01-12-2022
Subjects:
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Magnetic nanoparticle materials which could be used to remove tetracycline were confined seriously due to their poor stability and unsatisfactory reusability. Here, we facilely prepared novel zeolitic imidazolate framework-8 (ZIF-8) functionalized magnetic nanoparticles (Fe3O4@PDA-ZIF-8) adsorbent utilizing polydopamine as a bond to establish a connection between zeolitic imidazolate framework-8 and Fe3O4, which could improve the stability of magnetic nanoparticles and enhance the tetracycline adsorption capacity simultaneously. The prepared nanocomposites were characterized and their TC adsorption abilities under various experiment conditions (contact time, TC initial concentration and pH values) were also investigated. Experimental results proved that the prepared adsorbent showed superior TC adsorption capacities (92.01 mg/g at pH = 7). Further, the adsorption mechanisms were comprehensively studied and the prepared adsorbent showed satisfactory stability and reusability during the cycle experiment. Altogether, our findings provided a feasible way to design and construct functional magnetic MOF materials for enhancing tetracycline adsorption from wastewater. [Display omitted] •Fe3O4@PDA-ZIF-8 nanoparticles were first used as the adsorbent of tetracycline.•The maximum adsorption capacity of Fe3O4@PDA-ZIF-8 for TC was 92.01 mg/g.•Fe3O4@PDA-ZIF-8 can be recycled quickly and reused many times.•A detailed adsorption mechanism for TC in Fe3O4@PDA-ZIF-8 system was proposed.
Bibliography:ObjectType-Article-1
SourceType-Scholarly Journals-1
ObjectType-Feature-2
content type line 23
ISSN:0045-6535
1879-1298
DOI:10.1016/j.chemosphere.2022.136249