Syntheses and thermoanalytical studies of some schiff base polymers derived from 5,5′-methylene bis(2-hydroxyacetophenone)
Six Schiff base polymers poly 5,5′-methylenebis(2-hydroxyacetophenone)1,2-ethylenediimine (PHAen), poly[5,5′-methylenebis(2-hydroxyacetophenone)1,2-propylenediamine] (PHAPn), poly[5,5′-methylenebis (2-hydroxyacetophenone) 1,3-propyledenediamine] (PHAPR), poly[5,5′-methylenebis(2-hydroxyacetophenone)...
Saved in:
Published in: | European polymer journal Vol. 34; no. 1; pp. 133 - 135 |
---|---|
Main Authors: | , , |
Format: | Journal Article |
Language: | English |
Published: |
Oxford
Elsevier Ltd
1998
Elsevier |
Subjects: | |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | Six Schiff base polymers poly 5,5′-methylenebis(2-hydroxyacetophenone)1,2-ethylenediimine (PHAen), poly[5,5′-methylenebis(2-hydroxyacetophenone)1,2-propylenediamine] (PHAPn), poly[5,5′-methylenebis (2-hydroxyacetophenone) 1,3-propyledenediamine] (PHAPR), poly[5,5′-methylenebis(2-hydroxyacetophenone)
dl-stilbenediimine] (
dl-PHAS), poly[5,5′-methylenebis(2-hydroxyacetophenone)-
meso-stilbenediamine] (
meso-PHAS), and poly[5,5′-methylenebis(2-hydroxyacetophenone)azine] (PHAH) have been prepared by polycondensation of 5,5′-methylenebis(2-hydroxyacetophenone (MHA) with ethylenediamine,
dl-stilbenediamine
meso-stilbenediamine or hydrazine. Each of the polymers has been characterized by elemental microanalysis, infrared and ultraviolet spectroscopy. Their thermogravimetry (TG) and differential thermal analysis (DTA) have been recorded and evaluated. The reduced viscosity of the polymers measured in tetrahydrofuran (THF), dimethylformamide (DMF) and dimethyl sulphoxide (DMSO) was found within 0.202–0.505 dl/g. |
---|---|
ISSN: | 0014-3057 1873-1945 |
DOI: | 10.1016/S0014-3057(97)00078-5 |