Reduction of golgohar ore with noncocking coal of shahrood
Reduction of Golgohar iron are with noncocking coal of Shahrood has been investigated at temperatures 850, 925 and 1000 deg C. Effects of time and also ore to cock ratios has been studied. It is believed that a chance of gaining higher reduction in shorter time is not undesirable.