Effect of Millisecond Annealing Temperature of Ni1-xPtx Si Formation on Leakage Current Characteristics of Static Random- Access Memory Cells
The importance of optimizing the millisecond annealing (MSA) temperature for Pt-doped NiSi (<inline-formula> <tex-math notation="LaTeX">{\mathrm {Ni}}_{{1}-{x}} </tex-math></inline-formula>Pt x Si) contact formation was highlighted by implementing and characterizing...
Saved in:
Published in: | IEEE transactions on electron devices Vol. 66; no. 1; pp. 389 - 394 |
---|---|
Main Authors: | , , , , , , , , |
Format: | Journal Article |
Language: | English |
Published: |
IEEE
01-01-2019
|
Subjects: | |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | The importance of optimizing the millisecond annealing (MSA) temperature for Pt-doped NiSi (<inline-formula> <tex-math notation="LaTeX">{\mathrm {Ni}}_{{1}-{x}} </tex-math></inline-formula>Pt x Si) contact formation was highlighted by implementing and characterizing the <inline-formula> <tex-math notation="LaTeX">{\mathrm {Ni}}_{{1}-{x}} </tex-math></inline-formula>Pt x Si films in the static random-access memory (SRAM) cells fabricated with a 28-nm design rule. MSA at 750 °C-900 °C effectively reduced the junction leakage current compared to that with the conventional rapid thermal annealing, because of its efficient suppression of Ni diffusion in the junction region. Moreover, with an increase in the MSA temperature, the beneficial effects of maintaining a low junction leakage, such as interface flattening and grain size increase, were observed. However, the increase in the MSA temperature deteriorated the statistical distribution of the standby leakage current of the SRAM cells by producing more encroachment and spiking defects; this was attributed to the build-up of a high initial film stress and large stress relaxation during the subsequent back-end processes. |
---|---|
ISSN: | 0018-9383 1557-9646 |
DOI: | 10.1109/TED.2018.2878871 |