Preparation and anisotropic thermoelectric properties in misfit cobaltite thin films
We have investigated the control of crystal orientation in misfit layered cobaltite A/sub 3/Co/sub 4/O/sub 9/ (A=Ca, Sr) thin films and succeeded in growing epitaxial films with c-axis orientation perpendicular and parallel to the substrate surface by rf-planar magnetron sputtering. Anisotropic tran...
Saved in:
Published in: | ICT 2005. 24th International Conference on Thermoelectrics, 2005 pp. 288 - 291 |
---|---|
Main Authors: | , , , , |
Format: | Conference Proceeding |
Language: | English |
Published: |
IEEE
2005
|
Subjects: | |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | We have investigated the control of crystal orientation in misfit layered cobaltite A/sub 3/Co/sub 4/O/sub 9/ (A=Ca, Sr) thin films and succeeded in growing epitaxial films with c-axis orientation perpendicular and parallel to the substrate surface by rf-planar magnetron sputtering. Anisotropic transport properties (parallel to the CoO/sub 2/ layers (/spl par/) and perpendicular to the CoO/sub 2/ layers (/spl perp/)) were measured using the epitaxial films with c-axis parallel to the film plane. The resistivity for Sr/sub 3/Co/sub 4/O/sub 9/ parallel to the CoO/sub 2/ layers (/spl rho//sub /spl par//) is about 2.5 m/spl Omega/ cm at room temperature while that perpendicular to the CoO/sub 2/ layers (/spl rho//sub /spl perp//) is about 150 m/spl Omega/ cm. Sr/sub 3/Co/sub 4/O/sub 9/ has lower parallel and perpendicular resistivity than Ca/sub 3/Co/sub 4/O/sub 9/. As for thermoelectric properties of Sr/sub 3/Co/sub 4/O/sub 9/, Seebeck coefficient parallel to the CoO/sub 2/ layers (S/sub /spl par//) is 90 /spl mu/V/K and that perpendicular to the CoO/sub 2/ layers (S/sub /spl perp//) is 30 /spl mu/V/K at room temperature. The power factor parallel to the CoO/sub 2/ layers is calculated to be 3/spl times/10/sup -4/ W/mK/sup 2/, about two times higher than that for Ca/sub 3/Co/sub 4/O/sub 9/. The anisotropic value of resistivity for Ca/sub 3/Co/sub 4/O/sub 9/ and Sr/sub 3/Co/sub 4/O/sub 9/ is about 40 and 60, respectively, and that of Seebeck Coefficient is similarly about 3. |
---|---|
ISBN: | 0780395522 9780780395527 |
ISSN: | 1094-2734 |
DOI: | 10.1109/ICT.2005.1519942 |