Use of cement dust in the manufacture of vitrified sewer pipes
Waste by-pass cement dust was added in different percentages ranging from 2% to 10% to a standard mix for sewer pipes manufacture, as a substitute for expensive feldspar. It was found that a mix consisting of 45% kaolin, 36% ball clay, 9% grog and 10% by-pass dust and fired at a temperature of 1300...
Saved in:
Published in: | Waste management (Elmsford) Vol. 24; no. 6; pp. 597 - 602 |
---|---|
Main Authors: | , , , |
Format: | Journal Article |
Language: | English |
Published: |
Oxford
Elsevier Ltd
2004
New York, NY Elsevier Science |
Subjects: | |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | Waste by-pass cement dust was added in different percentages ranging from 2% to 10% to a standard mix for sewer pipes manufacture, as a substitute for expensive feldspar. It was found that a mix consisting of 45% kaolin, 36% ball clay, 9% grog and 10% by-pass dust and fired at a temperature of 1300 °C for 4 h yielded samples that meet the standards. It was possible to reach a water absorption of 4%, a modulus of rupture of 7.8 MPa and a resistance to acids and alkalis conforming with standard values. A test pipe was fabricated by vacuum extrusion using the suggested composition and was found to withstand a hydraulic pressure of 14 MPa for one minute without the appearance of any cracks. |
---|---|
Bibliography: | ObjectType-Article-2 SourceType-Scholarly Journals-1 ObjectType-Feature-1 content type line 23 |
ISSN: | 0956-053X 1879-2456 |
DOI: | 10.1016/j.wasman.2004.01.007 |