Preparation of nanoporous Ni and Ni–Cu by dealloying of rolled Ni–Mn and Ni–Cu–Mn alloys
Nanoporous Ni, Ni–Cu and Cu with ligament sizes of 10–20 nm were fabricated by dealloying rolled Ni–Mn, Cu–Ni–Mn and Cu–Mn alloys, respectively. Unlike conventional Raney nickel composed of brittle Ni–Al intermetallic compounds, the initial alloys had good workability. Ni and Cu atoms formed a homog...
Saved in:
Published in: | Journal of alloys and compounds Vol. 485; no. 1; pp. 583 - 587 |
---|---|
Main Authors: | , |
Format: | Journal Article |
Language: | English |
Published: |
Kidlington
Elsevier B.V
19-10-2009
Elsevier |
Subjects: | |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | Nanoporous Ni, Ni–Cu and Cu with ligament sizes of 10–20
nm were fabricated by dealloying rolled Ni–Mn, Cu–Ni–Mn and Cu–Mn alloys, respectively. Unlike conventional Raney nickel composed of brittle Ni–Al intermetallic compounds, the initial alloys had good workability. Ni and Cu atoms formed a homogeneous solid solution in the nanoporous architecture. The ligament sizes of nanoporous Ni and Ni–Cu were smaller than that of nanoporous Cu, reflecting the difference between the surface diffusivities of Ni and Cu. |
---|---|
Bibliography: | ObjectType-Article-2 SourceType-Scholarly Journals-1 ObjectType-Feature-1 content type line 23 |
ISSN: | 0925-8388 1873-4669 |
DOI: | 10.1016/j.jallcom.2009.06.031 |