Effects of compression molding on meltability of uranium dendrites for ingot consolidation in a pyroprocess

Compression molding was carried out to enhance the meltability of uranium dendrites. Uranium dendrites were successfully compressed, increasing their bulk density more than 9 times from 1.1 to 10 g/cm 3 . The average bulk density was about 8.7 g/cm 3 which was almost half of the material density. Th...