Degradation of protective coatings of the Ni-M-Cr-Al-Y system due to sulfide-oxide corrosion
The results of testing corrosion resistance longevity in coatings of the Ni-M-Cr-Al-Y system at temperatures of 800, 850, and 900°C are given. The kinetic dependences of corrosion are determined, successive stages of the degradation of coatings are identified, and the effect of alloying coatings wit...
Saved in:
Published in: | Metal science and heat treatment Vol. 49; no. 11-12; pp. 585 - 588 |
---|---|
Main Author: | |
Format: | Journal Article |
Language: | English |
Published: |
New York
Springer Nature B.V
01-11-2007
|
Subjects: | |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | The results of testing corrosion resistance longevity in coatings of the Ni-M-Cr-Al-Y system at temperatures of 800, 850, and 900°C are given. The kinetic dependences of corrosion are determined, successive stages of the degradation of coatings are identified, and the effect of alloying coatings with chromium and aluminum on their degradation and durability is established.[PUBLICATION ABSTRACT] |
---|---|
Bibliography: | ObjectType-Article-2 SourceType-Scholarly Journals-1 ObjectType-Feature-1 content type line 23 |
ISSN: | 0026-0673 1573-8973 |
DOI: | 10.1007/s11041-007-0109-3 |