    High-temperature oxidation process of intermetallic compound Ti-42 at % Al by TAKASAKI, A, OJIMA, K, TANEDA, Y, HOSHIYA, T, MITSUHASHI, A

    Published in Journal of materials science (01-01-1993)
    “…The oxidation process of two-phase (Ti sub 3 Al and TiAl) intermetallic compound, Ti--42 at.% Al, in air at 1073 and 1273K has been investigated. The oxidation…”
    Get full text
    Journal Article
  2. 2

    Observations of dislocations in white tin using high-resolution electron microscopy by OJIMA, K, TANEDA, Y

    Published in Japanese Journal of Applied Physics (01-04-1988)
    “…End-on dislocations in white tin crystals have been examined using high-resolution electron microscopy. The experimental lattice images indicated the…”
    Get full text
    Journal Article
  3. 3

    An Arrangement of Boundary Dislocations in White Tin Observed by High-Resolution Electron Microscopy by Ojima, Kozo, Taneda, Youji

    Published in Japanese Journal of Applied Physics (01-03-1989)
    “…The core structures of end-on dislocations at a low angle tilt boundary in white tin have been observed using high-resolution electron microscopy (HREM). HREM…”
    Get full text
    Journal Article
  4. 4

    Thermal growth of thin oxide in Ge films and interfacial bond defects of oxygen by SUNADA, J, FUKUCHI, K.-I, TANEDA, Y, HIROSE, M

    “…Taking account of the high photoabsorption coefficient of Ge for 290 nm light, we investigate the thermal growth of thin oxide in Ge films by utilizing a…”
    Get full text
    Journal Article
  5. 5

    Microstructures and Recrystallization of Cold-Rolled Single Crystals of Pure Iron by Taneda, Youji

    Published in Japanese Journal of Applied Physics (01-01-1965)
    “…The substructures and recrystallization of the cold-rolled iron crystals with different initial orientations have been studied by transmission electron…”
    Get full text
    Journal Article
  6. 6

    Arrangement of Dislocations in Iron Crystals Stretched in Tension by Yamashita, Tadayoshi, Taneda, Youji

    Published in Japanese Journal of Applied Physics (01-05-1963)
    “…Piled-up dislocations and dislocations forming cell structure in iron crystals are examined by transmission electron microscopy. It is found that the piled-up…”
    Get full text
    Journal Article
  7. 7

    Hydride dissociation and hydrogen evolution behavior of electrochemically charged pure titanium by Takasaki, Akito, Furuya, Yoshio, Ojima, Kozo, Taneda, Youji

    Published in Journal of alloys and compounds (01-07-1995)
    “…A commercially pure α-titanium was electrochemically charged with hydrogen in a 5% H2SO4 solution at a current density of 5 kA m−2 for 14.4 ks (4 h), and the…”
    Get full text
    Journal Article
  8. 8
  9. 9

    Transmission Electron Microscopic Observations of Dislocations Resulting from Allotropic Transformation of Pure Iron by Yamashita, Tadayoshi, Taneda, Youji

    Published in Journal of the Physical Society of Japan (01-01-1962)
    “…The phenomena resulting from the allotropic transformation of thin foils as well as thick specimens (7/100 mm thickness) of pure iron were examined by…”
    Get full text
    Journal Article
  10. 10

    Dislocations in Pure Iron Foils Deformed by Bending by Yamashita, Tadayoshi, Taneda, Youji

    Published in Journal of the Physical Society of Japan (01-01-1960)
    “…Dislocations in a thin section of a pure iron foil deformed by bending have been observed by transmission electron microscopy. The parallel dislocations up to…”
    Get full text
    Journal Article
  11. 11

    Hydrogen uptake in titanium aluminides covered with oxide layers by TAKASAKI, A, FURUYA, Y, TANEDA, Y

    “…Two-phase (Ti3Al and TiAl) Ti-45Al and Ti-50Al (at. pct) alloys, which were preoxidized in static air at 1098 K for times between 900 s and 14.4 ks, were…”
    Get full text
    Conference Proceeding Journal Article
  12. 12
  13. 13

    Hydrogen evolution from cathodically charged two-phase (Ti3Al + TiAl) titanium aluminides by Takasaki, Akito, Furuya, Yoshio, Ojima, Kozo, Taneda, Youji

    Published in Journal of alloys and compounds (01-07-1995)
    “…Ti-45Al and Ti-50Al (at.%) titanium aluminides, whose microstructures consisted of Ti3Al (α2) and TiAl (γ), were cathodically hydrogen-charged in a 5% H2SO4…”
    Get full text
    Journal Article
  14. 14

    Hydrogen uptake in titanium aluminides in high pressure hydrogen by Takasaki, Akito, Furuya, Yoshio, Taneda, Youji

    “…The weight gains of Ti–25Al, Ti–45Al and Ti–53Al alloys, with typical single-phase Ti 3Al, two-phase Ti 3Al/TiAl (fully lamellar) and single-phase TiAl…”
    Get full text
    Journal Article
  15. 15

    High-temperature oxidation process of intermetallic compound Ti-42 at. pct Al by Takasaki, Akito, Ojima, Kozo, Taneda, Youji, HOSHIYA, TAIJI, Mitsuhashi, Akira

    Published in Journal of materials science (01-01-1993)
    “…The oxidation process of two-phase (Ti3Al and TiAl) intermetallic compound, Ti-42 at. pct Al, in air at 1073 and 1273 K has been investigated. The oxidation at…”
    Get full text
    Journal Article
  16. 16

    High-temperature oxidation of cathodically hydrogen-charged two-phase (Ti3Al, TiAl) titanium aluminides by TAKASAKI, A, OJIMA, K, TANEDA, Y

    “…Titanium aluminides with 42, 45, and 50 at. pct Al that had undergone cathodic hydrogen charging have been oxidized in atmospheric-pressure static air at 1170…”
    Get full text
    Journal Article
  17. 17

    Electron Microscopic Study on the Oxidation of beta -Tin Irradiated by Electron Beam by Ojima, K, Taneda, Y

    Published in Journal of materials science (01-01-1990)
    “…Effects of electron beam irradiation to beta -Sn thin foils have been studied using high-resolution electron microscopy. By the beam irradiation, the beta -Sn…”
    Get full text
    Journal Article
  18. 18
  19. 19

    Hydrogen solubility of two-phase (Ti 3Al + TiAl) titanium aluminides by Takasaki, Akito, Furuya, Yoshio, Ojima, Kozo, Taneda, Youji

    Published in Scripta metallurgica et materialia (01-06-1995)
    “…The absorpsion and desorpsion of hydrogen by the two-phase titanium aluminide system were studied. The aluminide alloys Ti-45Al and Ti-50Al (at.%) were…”