Search Results - "Shakeri, H R"

  • Showing 1 - 13 results of 13
Refine Results
  1. 1

    Microstructural evolution during transient liquid phase bonding of Inconel 738LC using AMS 4777 filler alloy by Jalilvand, V., Omidvar, H., Shakeri, H.R., Rahimipour, M.R.

    Published in Materials characterization (01-01-2013)
    “…IN-738LC nickel-based superalloy was joined by transient liquid phase diffusion bonding using AMS 4777 filler alloy. The bonding process was carried out at…”
    Get full text
    Journal Article
  2. 2

    A Study on the Effect of Process Parameters on the Properties of Joint in TLP-Bonded Inconel 738LC Superalloy by Jalilvand, V., Omidvar, H., Shakeri, H. R., Rahimipour, M. R.

    “…Optimization of transient liquid phase (TLP)-bonding variables is essential to achieve a joint free from deleterious intermetallic constituents and with…”
    Get full text
    Journal Article
  3. 3

    Influence of bonding variables on transient liquid phase bonding behavior of nickel based superalloy IN-738LC by Jalilvand, V., Omidvar, H., Rahimipour, M.R., Shakeri, H.R.

    Published in Materials in engineering (01-12-2013)
    “…The effect of process variables on the microstructure and properties of transient liquid phase (TLP) bonded IN-738LC superalloy was investigated using AMS 4776…”
    Get full text
    Journal Article
  4. 4

    Effect of alternative aging process on the fracture and interfacial properties of particulate Al2O3-Reinforced Al (6061) metal matrix composite by SHAKERI, H. R, WANG, Zhirui

    “…The effects of different aging processes on ductility, fracture, and interfacial properties in particulate Al2O3-reinforced Al (6061) MMCs were studied…”
    Get full text
    Journal Article
  5. 5

    Formability Enhancement of Galvanized IF-Steel TWB by Modification of Forming Parameters by Abbasi, M., Ketabchi, M., Shakeri, H. R., Hasannia, M. H.

    “…Tailor-welded blanks (TWBs) have numerous advantages over traditional blanks used in manufacturing, such as energy conservation and environment protection. Low…”
    Get full text
    Journal Article
  6. 6

    Optimization of heat treatment in cold-drawn 6063 aluminium tubes by Bourget, J.-P., Fafard, M., Shakeri, H.R., Côté, T.

    Published in Journal of materials processing technology (21-06-2009)
    “…The effect of heat treatment condition on mechanical properties and bendability of 6063 aluminium cold-drawn tubes was investigated. The standardized heat…”
    Get full text
    Journal Article
  7. 7

    Obtaining high formability of IF-galvanized steel tailor welded blanks by applying optimum CO2 laser welding parameters by Abbasi, M., Ketabchi, M., Shakeri, H. R., Shafaat, M. A.

    “…Tailor welded blanks are complex component designs tailor-made through welding of multiple metal sheets with different thicknesses, shapes and/or strengths…”
    Get full text
    Journal Article
  8. 8

    Obtaining high formability of IF-galvanized steel tailor welded blanks by applying optimum CO sub(2) laser welding parameters by Abbasi, M, Ketabchi, M, Shakeri, H R, Shafaat, M A

    “…Tailor welded blanks are complex component designs tailor-made through welding of multiple metal sheets with different thicknesses, shapes and/or strengths…”
    Get full text
    Journal Article
  9. 9

    Obtaining high formability of IF-galvanized steel tailor welded blanks by applying optimum CO 2 laser welding parameters by Abbasi, M., Ketabchi, M., Shakeri, H. R., Shafaat, M. A.

    “…Abstract Tailor welded blanks are complex component designs tailor-made through welding of multiple metal sheets with different thicknesses, shapes and/or…”
    Get full text
    Journal Article
  10. 10

    Effect of alternative aging process on the fracture and interfacial properties of participate Al sub 2 O sub 3 -reinforced Al (6061) metal matrix composite by Shakeri, H R, Wang, Z

    “…The effects of different aging processes on ductility, fracture, and interfacial properties in particulate Al sub 2 O sub 3 -reinforced Al (6061) metal-matrix…”
    Get full text
    Journal Article
  11. 11

    Effect of alternative aging process on the fracture and interfacial properties of particulate AI(2)O(3)-reinforced AI (6061) metal matrix composite by Shakeri, H R, Wang, Zhirui

    “…The effects of different aging processes on ductility, fracture, and interfacial properties in particulate Al2O3-reinforced Al (6061) metal-matrix composite…”
    Get full text
    Journal Article
  12. 12

    Weld Failure in Formability Testing of Aluminum Tailor Welded Blanks by Shakeri, H. R., Lee, Y., Worswick, M. J., Feng, F., Christy, W., Clarke, J. A.

    Published in SAE transactions (01-01-2001)
    “…The present work investigates weld failure modes during formability tests of multi-gauge aluminum Tailor Welded Blanks (TWBs). The limiting dome height test is…”
    Get full text
    Journal Article
  13. 13

    Study of damage initiation and fracture in aluminum tailor welded blanks made via different welding techniques by Shakeri, H.R., Buste, A., Worswick, M.J., Clarke, J.A., Feng, F., Jain, M., Finn, M.

    Published in Journal of light metals (01-05-2002)
    “…The present paper addresses microstructural evaluation of failure in multi-gauge aluminum alloy tailor welded blanks (TWBs), welded using non-vacuum electron…”
    Get full text
    Journal Article