Search Results - "Sakai, Munetoshi"

Refine Results
  1. 1

    Droplet viscosity effects on dynamic hydrophobicity of a solid–liquid bulk composite prepared from porous glass by Yokoyama, Kota, Sakai, Munetoshi, Isobe, Toshihiro, Matsushita, Sachiko, Nakajima, Akira

    Published in Journal of materials science (01-01-2017)
    “…Hydrophobic porous glass plates were prepared by coating a fluorosilane (FAS17) onto a commercial porous glass (average pore size, approx. 1 μm). Based on the…”
    Get full text
    Journal Article
  2. 2

    Effect of Surface Structure on the Sustainability of an Air Layer on Superhydrophobic Coatings in a Water−Ethanol Mixture by Sakai, Munetoshi, Yanagisawa, Tomoki, Nakajima, Akira, Kameshima, Yoshikazu, Okada, Kiyoshi

    Published in Langmuir (06-01-2009)
    “…Using a laser beam and its reflection, we evaluated surface air layers on two superhydrophobic coatings with different roughnesses (R a = 1900 and 74 nm) in a…”
    Get full text
    Journal Article
  3. 3

    Theoretical Kinetic Analysis of Heterogeneous Photocatalysis by TiO2 Nanotube Arrays: the Effects of Nanotube Geometry on Photocatalytic Activity by Liu, Baoshun, Nakata, Kazuya, Liu, Shanhu, Sakai, Munetoshi, Ochiai, Tsuyoshi, Murakami, Taketoshi, Takagi, Katsuhiko, Fujishima, Akira

    Published in Journal of physical chemistry. C (05-04-2012)
    “…TiO2 nanotube arrays are important functional materials in photocatalysis. Compared with other TiO2 materials, the geometrical parameters of the nanotubes in…”
    Get full text
    Journal Article
  4. 4

    Factors Affecting UV-Induced Superhydrophilic Conversion of a TiO2 Surface by Emeline, Alexei V, Rudakova, Aida V, Sakai, Munetoshi, Murakami, Taketoshi, Fujishima, Akira

    Published in Journal of physical chemistry. C (13-06-2013)
    “…The present study explored the effects of several factors (wetting, light intensity, spectral variation of the actinic light, heating, and surface acidity) on…”
    Get full text
    Journal Article
  5. 5

    Carbon dioxide adsorption properties of K-Al-Fe–based oxides prepared from a porous polymer monolith template by Ikeue, Keita, Suzuki, Masashige, Yoshimoto, Daisuke, Usukawa, Ryutaro, Sakai, Munetoshi, Vagvala, Tarun Chand, Kalousek, Vit

    Published in Journal of solid state chemistry (01-06-2019)
    “…K-Al-Fe–based oxides with bimodal pores in the meso- and macro-size range were synthesized using spherical porous polymer monolith templates containing…”
    Get full text
    Journal Article
  6. 6

    Preparation and hydrophobicity of solid–liquid bulk composite using porous glass and fluorinated oil by Takada, Yasuhiro, Sakai, Munetoshi, Isobe, Toshihiro, Matsushita, Sachiko, Nakajima, Akira

    Published in Journal of materials science (01-12-2015)
    “…Hydrophobic porous glass plates were prepared by coating a fluorosilane (FAS17) onto a commercial porous glass (average pore size, approx. 1 μm) with surface…”
    Get full text
    Journal Article
  7. 7

    Synthesis and characterization of metal-diaminobipyridine complexes as low-cost co-catalysts for photo-sensitized hydrogen evolution by Chand Vagvala, Tarun, Ooyabe, Takashi, Sakai, Munetoshi, Funasako, Yusuke, Inokuchi, Makoto, Kurashige, Wataru, Negishi, Yuichi, Kalousek, Vit, Ikeue, Keita

    Published in Inorganica Chimica Acta (01-10-2018)
    “…[Display omitted] •Novel 4,4′-diamino-2,2′-bipyridyl complexes of Co(III), Ni(II), and Cu(II) were synthesized.•The activities of above complexes for…”
    Get full text
    Journal Article
  8. 8

    Preparation and Photocatalytic Activity of Robust Titania Monoliths for Water Remediation by Nakata, Kazuya, Kagawa, Tomoya, Sakai, Munetoshi, Liu, Shanhu, Ochiai, Tsuyoshi, Sakai, Hideki, Murakami, Taketoshi, Abe, Masahiko, Fujishima, Akira

    Published in ACS applied materials & interfaces (13-02-2013)
    “…TiO2 monoliths were prepared, characterized, and evaluated for photocatalytic performance. The TiO2 monoliths were found to have an interconnected void lattice…”
    Get full text
    Journal Article
  9. 9

    Comparative study of the impact and sliding behavior of water droplets on two different hydrophobic silane coatings by Nakajima, Akira, Miyamoto, Takumi, Sakai, Munetoshi, Isobe, Toshihiro, Matsushita, Sachiko

    Published in Applied surface science (15-02-2014)
    “…•Smooth hydrophobic silane (ODS and FAS17) coatings were prepared.•Impact and sliding behaviors of water droplets on the coatings were investigated.•Droplets…”
    Get full text
    Journal Article
  10. 10

    Direct Observation of Internal Fluidity in a Water Droplet during Sliding on Hydrophobic Surfaces by Sakai, Munetoshi, Song, Jeong-Hwan, Yoshida, Naoya, Suzuki, Shunsuke, Kameshima, Yoshikazu, Nakajima, Akira

    Published in Langmuir (23-05-2006)
    “…In the current study, we used a high-speed camera system with particle image velocimetry to observe the internal fluidity of water droplets during sliding. The…”
    Get full text
    Journal Article
  11. 11

    Adhesion and Friction Force on Various Smooth Hydrophobic Silane Coatings by Miyamoto, Takumi, Sakai, Munetoshi, Isobe, Toshihiro, Matsushita, Sachiko, Nakajima, Akira

    Published in Chemistry letters (05-05-2015)
    “…Various smooth hydrophobic silane coatings were prepared on a Si substrate using CVD. Then adhesion and friction force for these coatings were evaluated using…”
    Get full text
    Journal Article
  12. 12

    Removing an Air Layer from a Superhydrophobic Surface in Flowing Water by Sakai, Munetoshi, Nakajima, Akira, Fujishima, Akira

    Published in Chemistry letters (05-05-2010)
    “…The removal of a surface air layer from a superhydrophobic coating in flowing water was evaluated using a laser beam and a high-speed camera. It proceeded via…”
    Get full text
    Journal Article
  13. 13

    Evaporation Behavior of Microliter- and Sub-nanoliter-Scale Water Droplets on Two Different Fluoroalkylsilane Coatings by Furuta, Tsutomu, Sakai, Munetoshi, Isobe, Toshihiro, Nakajima, Akira

    Published in Langmuir (20-10-2009)
    “…The evaporation behavior of microliter (2.0 μL) and subnanoliter (0.8 nL) scale water droplets was investigated on two smooth hydrophobic and hydrophilic…”
    Get full text
    Journal Article
  14. 14

    UV/Thermally Driven Rewritable Wettability Patterns on TiO2−PDMS Composite Films by Nakata, Kazuya, Kimura, Hiroaki, Sakai, Munetoshi, Ochiai, Tsuyoshi, Sakai, Hideki, Murakami, Taketoshi, Abe, Masahiko, Fujishima, Akira

    Published in ACS applied materials & interfaces (01-09-2010)
    “…Composite films of TiO2 and polydimethylsiloxane (PDMS) are prepared by a sol−gel method, cured with UV irradiation, and then treated in hot water to…”
    Get full text
    Journal Article
  15. 15

    Bending motion of a polyacrylamide/graphite fiber driven by a wide range of light from UV to NIR by Nakata, Kazuya, Sakai, Munetoshi, Ochiai, Tsuyoshi, Murakami, Taketoshi, Fujishima, Akira

    Published in Materials letters (01-05-2012)
    “…Photomechanical motion of a polyacrylamide-based fiber containing graphite as a dye was observed upon illumination with a wide range of light from UV to NIR…”
    Get full text
    Journal Article
  16. 16

    Image analysis system for evaluating sliding behavior of a liquid droplet on a hydrophobic surface by Sakai, Munetoshi, Hashimoto, Ayako, Yoshida, Naoya, Suzuki, Shunsuke, Kameshima, Yoshikazu, Nakajima, Akira

    Published in Review of scientific instruments (01-04-2007)
    “…An analysis system was developed to evaluate the sliding behavior of a liquid droplet on a hydrophobic surface. This system enables continuous and simultaneous…”
    Get more information
    Journal Article
  17. 17

    Comparative study of the dynamic hydrophobicity of fluoroalkylsilane coatings tilted at acute and obtuse angles by Higashino, Yuta, Takahashi, Hirokazu, Sakai, Munetoshi, Isobe, Toshihiro, Matsushita, Sachiko, Nakajima, Akira

    Published in JCT research (01-07-2018)
    “…The relation between surface homogeneity and internal fluidity for a droplet sliding on a surface tilted at acute and obtuse angles was investigated using two…”
    Get full text
    Journal Article
  18. 18

    Visible Light Responsive Electrospun TiO2 Fibers Embedded with WO3 Nanoparticles by Nakata, Kazuya, Liu, Baoshun, Goto, Yuri, Ochiai, Tsuyoshi, Sakai, Munetoshi, Sakai, Hideki, Murakami, Taketoshi, Abe, Masahiko, Fujishima, Akira

    Published in Chemistry letters (05-10-2011)
    “…TiO2–WO3 composite fibers were prepared by electrospinning. The fibers have an average diameter of 1.0 µm. The XRD pattern of the TiO2–WO3 composite fibers…”
    Get full text
    Journal Article
  19. 19

    Fabrication and characterization of self-organized porous TiO2 particle layers by Nakata, Kazuya, Sakai, Munetoshi, Ochiai, Tsuyoshi, Murakami, Taketoshi, Takagi, Katsuhiko, Fujishima, Akira

    Published in Materials letters (01-03-2012)
    “…Self-organized porous TiO2 particle layers were fabricated by simple calcination of a Ti substrate in air. The TiO2 particle layers were formed by calcination…”
    Get full text
    Journal Article
  20. 20

    Slipping and Rolling Ratio of Sliding Acceleration for a Water Droplet Sliding on Fluoroalkylsilane Coatings of Different Roughness by Suzuki, Shunsuke, Nakajima, Akira, Sakai, Munetoshi, Sakurada, Yuu, Yoshida, Naoya, Hashimoto, Ayako, Kameshima, Yoshikazu, Okada, Kiyoshi

    Published in Chemistry letters (05-01-2008)
    “…The effect of surface roughness on the internal fluidity of a water droplet during sliding on an inclined Si surface treated fluoroalkylsilane (FAS) was…”
    Get full text
    Journal Article