  1. 1

    Indentation brittleness of ceramics : a fresh approach by QUINN, J. B, QUINN, G. D

    Published in Journal of materials science (15-08-1997)
    “…The hardness and brittleness of ceramic materials are interrelated. Hard materials are more apt to fracture in the vicinity of an indentation during a hardness…”
    Get full text
    Journal Article
  2. 2

    On edge chipping testing and some personal perspectives on the state of the art of mechanical testing by Quinn, G.D

    Published in Dental materials (01-01-2015)
    “…Highlights • Edge chipping tests with simple rectangular test blocks evaluate a materials resistance to chipping. • Materials may be ranked for their chipping…”
    Get full text
    Journal Article
  3. 3

    Chipping fracture resistance of dental CAD/CAM restorative materials: Part I – Procedures and results by Quinn, G.D, Giuseppetti, A.A, Hoffman, K.H

    Published in Dental materials (01-05-2014)
    “…Abstract Objective The edge chipping test was used to measure the fracture resistance of CAD/CAM dental restoration ceramics and resin composites. Methods An…”
    Get full text
    Journal Article
  4. 4

    Investigation into the Mechanical Cause of Failure of Neutron Guide NG-2 at the NIST Research Reactor by ZILCHA, O, QUINN, G. D, ROWE, J. M, PIERCE, D. J

    Published in Journal of failure analysis and prevention (01-12-2012)
    “…This study investigates the fractures that occurred in a glass structure used to carry neutrons from a cold source in the NIST reactor into an experimental…”
    Get full text
    Journal Article
  5. 5

    ON THE NATURE OF MACHINING CRACKS IN GROUND CERAMICS: PART I: SRBSN STRENGTHS AND FRACTOGRAPHIC ANALYSIS by Quinn, G. D., Ives, L. K., Jahanmir, S.

    Published in Machining science and technology (01-06-2005)
    “…Machining cracks in ground sintered reaction-bonded silicon nitride (SRBSN) rods and bars were analyzed by fractographic techniques. Grinding flaw sizes were…”
    Get full text
    Journal Article
  6. 6

    Chipping fracture resistance of dental CAD/CAM restorative materials: Part 2. Phenomenological model and the effect of indenter type by Quinn, G.D, Giuseppetti, A.A, Hoffman, K.H

    Published in Dental materials (01-05-2014)
    “…Abstract The edge chipping resistances of six CAD/CAM dental restoration materials are analyzed and correlated to other mechanical properties. A new quadratic…”
    Get full text
    Journal Article
  7. 7

    Chipping fracture resistance of denture tooth materials by Quinn, G.D, Giuseppetti, A.A, Hoffman, K.H

    Published in Dental materials (01-05-2014)
    “…Abstract Objective The applicability of the edge chipping method to denture tooth materials was assessed. These are softer materials than those usually tested…”
    Get full text
    Journal Article
  8. 8

    Dynamic Compression Strength of Ceramics: What was Learned from an Interlaboratory Round Robin Exercise? by Swab, J. J., Chen, W., Hogan, J., Liao, H., Lo, C., Mates, S., Meredith, C., Pittari, J. J., Rhorer, R., Quinn, G. D.

    Published in Journal of dynamic behavior of materials (01-03-2021)
    “…The dynamic compressive strength of a commercial alumina was determined by five participants using the Split-Hopkinson pressure bar (SHPB) method with a…”
    Get full text
    Journal Article
  9. 9

    Fracture toughness ( KIc) of a dental porcelain determined by fractographic analysis by Scherrer, S.S., Robert Kelly, J., Quinn, G.D., Xu, K.

    Published in Dental materials (01-09-1999)
    “…Objectives: Fractographic analysis of indentation cracks is performed following flexure testing as part of the ASTM (1999) standard for fracture toughness, K…”
    Get full text
    Journal Article
  10. 10

    Dugbe virus ovarian tumour domain interferes with ubiquitin/ISG15-regulated innate immune cell signalling by Bakshi, S, Holzer, B, Bridgen, A, McMullan, G, Quinn, D G, Baron, M D

    Published in Journal of general virology (01-02-2013)
    “…The ovarian tumour (OTU) domain of the nairovirus L protein has been shown to remove ubiquitin and interferon-stimulated gene 15 protein (ISG15) from host cell…”
    Get full text
    Journal Article
  11. 11

    Bridging stresses in sintered reaction-bonded Si3N4 from COD measurements by Fett, T, Munz, D, Kounga Njiwa, A B, Rodel, J, Quinn, G D

    Published in Journal of the European Ceramic Society (01-01-2005)
    “…Crack opening displacement (COD) measurements on a sintered reaction-bonded Si3N4 ceramic obtained in bending tests with edge-V-notched specimens were…”
    Get full text
    Journal Article
  12. 12

    An inset CT specimen for evaluating fracture in small samples of material by Yahyazadehfar, M., Nazari, A., Kruzic, J.J., Quinn, G.D., Arola, D.

    “…In evaluations on the fracture behavior of hard tissues and many biomaterials, the volume of material available to study is not always sufficient to apply a…”
    Get full text
    Journal Article
  13. 13

    Fatigue of zirconia and dental bridge geometry: Design implications by Quinn, G.D, Studart, A.R, Hebert, C, VerHoef, J.R, Arola, D

    Published in Dental materials (01-12-2010)
    “…Abstract Zirconia is currently used as a framework material for posterior all-ceramic bridges. While the majority of research efforts have focused on the…”
    Get full text
    Journal Article
  14. 14

    ON THE NATURE OF MACHINING CRACKS IN GROUND CERAMICS: PART II, COMPARISON TO OTHER SILICON NITRIDES AND DAMAGE MAPS by Quinn, G. D., Ives, L. K., Jahanmir, S.

    Published in Machining science and technology (01-06-2005)
    “…The size and severity of grinding machining cracks in a sintered reaction bonded silicon nitride are compared to data for other silicon nitrides. Crack sizes…”
    Get full text
    Journal Article
  15. 15

    Weibull Strength Scaling for Standardized Rectangular Flexure Specimens by Quinn, George D.

    Published in Journal of the American Ceramic Society (01-03-2003)
    “…Formulas for the effective volumes and effective surfaces for rectangular bars loaded in flexure are reviewed. The ratio of strengths from any two…”
    Get full text
    Journal Article
  16. 16

    Effect of Precrack "Halos" on Fracture Toughness Determined by the Surface Crack in Flexure Method by Swab, Jeffrey J., Quinn, George D.

    Published in Journal of the American Ceramic Society (01-09-1998)
    “…The surface crack in flexure method, which is used to determine the fracture toughness of dense ceramics, necessitates the measurement of precrack sizes by…”
    Get full text
    Journal Article
  17. 17

    Anomalous Defects and Dynamic Failure of Armor Ceramics by Bakas, M.P., Greenhut, V.A., Niesz, D.E., Quinn, G. D., McCauley, J. W., Wereszczak, A. A., Swab, J. J.

    “…The ballistic performance of state‐of‐the‐art silicon carbide armor material can exhibit a fairly wide variability in certain test configurations, which, it is…”
    Get full text
    Journal Article
  18. 18

    Fracture Toughness of Veneering Ceramics for Fused to Metal (PFM) and Zirconia Dental Restorative Materials by Quinn, Janet B, Quinn, George D, Sundar, Veeraraghaven

    “…Veneering ceramics designed to be used with modern zirconia framework restorations have been reported to fracture occasionally in vivo. The fracture toughness…”
    Get full text
    Journal Article
  19. 19

    Fracture toughness of advanced ceramics at room temperature by Quinn, George D., Salem, Jonathan, Bar-On, Isa, Cho, Kyu, Foley, Michael, Fang, HO

    “…Results of round-robin fracture toughness tests on advanced ceramics are reported. A gas-pressure silicon nitride and a zirconia-toughened alumina were tested…”
    Get full text
    Journal Article
  20. 20

    Weibull Effective Volumes and Surfaces for Cylindrical Rods Loaded in Flexure by Quinn, George D.

    Published in Journal of the American Ceramic Society (01-03-2003)
    “…Formulas are given for the effective volumes and effective surfaces for cylindrical rods that have been loaded in flexure. Strength scaling for specimen size…”