Effect of Composition and Thickness of Organosilicate Coatings on the Arc Welding Process

The behavior and destruction features of organosilicate coatings and its components during electric arc welding / surfacing were considered. The effects of the organosilicate compositions (OS-51-03 (green), OS-51-03 (gray), OS-56-22 (gray) and OS-82-01 (green)), its thicknesses and influence of weld...

Full description

Saved in:
Bibliographic Details
Published in:Russian journal of applied chemistry Vol. 92; no. 9; pp. 1274 - 1283
Main Authors: Zhabrev, L. A., Chuppina, S. V., Panchenko, O. V., Repin, I. L., Popovisch, A. A.
Format: Journal Article
Language:English
Published: Moscow Pleiades Publishing 01-09-2019
Springer Nature B.V
Subjects:
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:The behavior and destruction features of organosilicate coatings and its components during electric arc welding / surfacing were considered. The effects of the organosilicate compositions (OS-51-03 (green), OS-51-03 (gray), OS-56-22 (gray) and OS-82-01 (green)), its thicknesses and influence of welding parameters on the porosity and the presence of the other defects in the weld metal were investigated. Gas pores, wormholes and nonmetallic inclusions are found as typical defects in the welded joints of organosilicate coated metal. Defects formed in the weld pool crystallization zone during the physical, chemical and metallurgical processes when the coating destruction products interact with a liquid metal.
ISSN:1070-4272
1608-3296
DOI:10.1134/S1070427219090131