Search Results - "Pierce, D.T"

Refine Results
  1. 1

    The influence of stacking fault energy on the microstructural and strain-hardening evolution of Fe–Mn–Al–Si steels during tensile deformation by Pierce, D.T., Jiménez, J.A., Bentley, J., Raabe, D., Wittig, J.E.

    Published in Acta materialia (01-11-2015)
    “…[Display omitted] Understanding the relationship between the stacking-fault energy (SFE), deformation mechanisms, and strain-hardening behavior is important…”
    Get full text
    Journal Article
  2. 2

    Effects of strain rate on mechanical properties and deformation behavior of an austenitic Fe-25Mn-3Al-3Si TWIP-TRIP steel by Benzing, J.T., Poling, W.A., Pierce, D.T., Bentley, J., Findley, K.O., Raabe, D., Wittig, J.E.

    “…The effects of quasi-static and low-dynamic strain rate (ε̇ = 10−4 /s to ε̇ = 102 /s) on tensile properties and deformation mechanisms were studied in a…”
    Get full text
    Journal Article
  3. 3

    Characterization of transition carbides in quench and partitioned steel microstructures by Mössbauer spectroscopy and complementary techniques by Pierce, D.T., Coughlin, D.R., Williamson, D.L., Clarke, K.D., Clarke, A.J., Speer, J.G., De Moor, E.

    Published in Acta materialia (01-05-2015)
    “…Quenching and partitioning (Q&P) produces steel microstructures with martensite and austenite that exhibit promising property combinations for third generation…”
    Get full text
    Journal Article
  4. 4

    Temperature effect on deformation mechanisms and mechanical properties of a high manganese C+N alloyed austenitic stainless steel by Mosecker, L., Pierce, D.T., Schwedt, A., Beighmohamadi, M., Mayer, J., Bleck, W., Wittig, J.E.

    “…Recently developed high-manganese stainless Fe–Cr–Mn–CN steels exhibit an exceptional combination of strength and ductility and show great promise for…”
    Get full text
    Journal Article
  5. 5

    Evaluation of thermal processing and properties of 422 martensitic stainless steel for replacement of 4140 steel in diesel engine pistons by Pierce, D.T., Muralidharan, G., Trofimov, A., Torres, J., Wang, H., Haynes, J.A., Sebeck, K., Gingrich, E., Byrd, G., Tess, M.

    Published in Materials & design (01-02-2022)
    “…[Display omitted] •Tempering from 600 to 700 °C substantially modifies elevated temperature strength of 422 but has no significant influence on thermal…”
    Get full text
    Journal Article
  6. 6
  7. 7

    Effect of roughness, frustration, and antiferromagnetic order on magnetic coupling of Fe/Cr multilayers by Pierce, D.T, Unguris, J, Celotta, R.J, Stiles, M.D

    “…The interplay between interfacial disorder and the antiferromagnetic order in Cr leads to complex behavior in Fe/Cr multilayers. Measurements of interlayer…”
    Get full text
    Journal Article
  8. 8

    Spin nomenclature for semiconductors and magnetic metals by Jonker, B.T., Hanbicki, A.T., Pierce, D.T., Stiles, M.D.

    “…The different conventions used in the semiconductor and magnetic metals communities can cause confusion in the context of spin polarization and transport in…”
    Get full text
    Journal Article
  9. 9

    The influence of manganese content on the stacking fault and austenite/ε-martensite interfacial energies in Fe–Mn–(Al–Si) steels investigated by experiment and theory by Pierce, D.T., Jiménez, J.A., Bentley, J., Raabe, D., Oskay, C., Wittig, J.E.

    Published in Acta materialia (15-04-2014)
    “…The stacking fault and interfacial energies of three transformation- and twinning-induced plasticity steels (TRIP/TWIP) (Fe–22/25/28Mn–3Al–3Si wt.%) were…”
    Get full text
    Journal Article
  10. 10

    Microstructural evolution during quenching and partitioning of 0.2C-1.5Mn-1.3Si steels with Cr or Ni additions by Pierce, D.T., Coughlin, D.R., Clarke, K.D., De Moor, E., Poplawsky, J., Williamson, D.L., Mazumder, B., Speer, J.G., Hood, A., Clarke, A.J.

    Published in Acta materialia (01-06-2018)
    “…The influence of Cr and Ni additions and quench and partition (Q&P) processing parameters on the microstructural development, including carbide formation and…”
    Get full text
    Journal Article
  11. 11

    Hot deformation behavior of an industrially cast large grained low density austenitic steel by Pierce, D.T., Field, D.M., Limmer, K.R., Muth, T., Sebeck, K.M.

    “…Hot compression testing was performed on specimens of an Fe–30Mn–9Al–1Si-0.9C-0.5Mo wt.% low density steel which were extracted from an industrial casting with…”
    Get full text
    Journal Article
  12. 12

    Simultaneous control of the Dzyaloshinskii-Moriya interaction and magnetic anisotropy in nanomagnetic trilayers by Balk, A L, Kim, K-W, Pierce, D T, Stiles, M D, Unguris, J, Stavis, S M

    Published in Physical review letters (17-08-2017)
    “…Magneto-optical Kerr effect (MOKE) microscopy measurements of magnetic bubble domains demonstrate that Ar^{+} irradiation around 100 eV can tune the…”
    Get full text
    Journal Article
  13. 13

    Quantitative investigation into the influence of temperature on carbide and austenite evolution during partitioning of a quenched and partitioned steel by Pierce, D.T., Coughlin, D.R., Williamson, D.L., Kähkönen, J., Clarke, A.J., Clarke, K.D., Speer, J.G., De Moor, E.

    Published in Scripta materialia (01-08-2016)
    “…The influence of partitioning temperature on microstructural evolution during quenching and partitioning was investigated in a 0.38C1.54Mn1.48Si wt.% steel…”
    Get full text
    Journal Article
  14. 14

    Stacking fault energy measurements of Fe–Mn–Al–Si austenitic twinning-induced plasticity steels by Pierce, D.T., Bentley, J., Jiménez, J.A., Wittig, J.E.

    Published in Scripta materialia (01-05-2012)
    “…Since the stacking fault energy significantly influences the deformation mechanisms of Fe–Mn–Al–Si twinning-induced plasticity steels, two methods for its…”
    Get full text
    Journal Article
  15. 15

    Exchange coupling in magnetic multilayers grown on iron whiskers by Unguris, J, Celotta, R.J, Tulchinsky, D.A, Pierce, D.T

    “…Meaningful tests of theoretical predictions of magnetic multilayer properties require the fabrication of multilayers with nearly the same atomic scale…”
    Get full text
    Journal Article Conference Proceeding
  16. 16
  17. 17

    End States in One-Dimensional Atom Chains by Crain, J. N, Pierce, D. T

    “…End states--the zero-dimensional analogs of the two-dimensional states that occur at a crystal surface--were observed at the ends of one-dimensional atom…”
    Get full text
    Journal Article
  18. 18

    The influence of temperature on the strain-hardening behavior of Fe-22/25/28Mn-3Al-3Si TRIP/TWIP steels by Pierce, D.T., Benzing, J.T., Jiménez, J.A., Hickel, T., Bleskov, I., Keum, J., Raabe, D., Wittig, J.E.

    Published in Materialia (01-05-2022)
    “…The influence of temperature and stacking fault energy (SFE) on the strain-hardening behavior and critical resolved shear stress for twinning was investigated…”
    Get full text
    Journal Article
  19. 19

    Simultaneous measurement of magnetic vortex polarity and chirality using scanning electron microscopy with polarization analysis (SEMPA) by Chung, S.-H., Pierce, D.T., Unguris, J.

    Published in Ultramicroscopy (01-02-2010)
    “…The magnetic vortex structure is an equilibrium configuration frequently found in patterned magnetic nanostructures. It is characterized by an in-plane curling…”
    Get full text
    Journal Article
  20. 20