    Effect of rare earth additions on microstructure and texture development of magnesium alloy sheets by Hantzsche, K., Bohlen, J., Wendt, J., Kainer, K.U., Yi, S.B., Letzig, D.

    Published in Scripta materialia (01-10-2010)
    “…Rare earth elements or yttrium can weaken the strong basal textures of magnesium sheets and are of interest for the improvement of sheet formability. The…”
    Get full text
    Journal Article
  2. 2

    Microstructure, mechanical and corrosion properties of Mg–Dy–Gd–Zr alloys for medical applications by Yang, L., Huang, Y., Feyerabend, F., Willumeit, R., Mendis, C., Kainer, K.U., Hort, N.

    Published in Acta biomaterialia (01-11-2013)
    “…In previous investigations, a Mg–10Dy (wt.%) alloy with a good combination of corrosion resistance and cytocompatibility showed great potential for use as a…”
    Get full text
    Journal Article
  3. 3

    Waste Mg-Al based alloys for hydrogen storage by Hardian, R., Pistidda, C., Chaudhary, A.-L., Capurso, G., Gizer, G., Cao, H., Milanese, C., Girella, A., Santoru, A., Yigit, D., Dieringa, H., Kainer, K.U., Klassen, T., Dornheim, M.

    Published in International journal of hydrogen energy (23-08-2018)
    “…Magnesium has been studied as a potential hydrogen storage material for several decades because of its relatively high hydrogen storage capacity, fast sorption…”
    Get full text
    Journal Article
  4. 4

    The role of anions in the formation and corrosion resistance of the plasma electrolytic oxidation coatings by Ghasemi, A., Raja, V.S., Blawert, C., Dietzel, W., Kainer, K.U.

    Published in Surface & coatings technology (01-01-2010)
    “…Combination of KOH with each of Na 2SiO 3, Na 3PO 4 and NaAlO 2, formed three different coating solutions to produce plasma electrolytic oxidation (PEO)…”
    Get full text
    Journal Article
  5. 5

    Study of the structure and corrosion behavior of PEO coatings on AM50 magnesium alloy by electrochemical impedance spectroscopy by Ghasemi, A., Raja, V.S., Blawert, C., Dietzel, W., Kainer, K.U.

    Published in Surface & coatings technology (25-04-2008)
    “…In this work coatings were developed on the surface of AM50 magnesium alloy using four different electrolytes containing 10 wt.% each of K 3PO 4 and Na 3PO 4…”
    Get full text
    Journal Article
  6. 6

    Fatigue of Magnesium Alloys by Potzies, C., Kainer, K.U.

    Published in Advanced engineering materials (01-05-2004)
    “…Magnesium alloys show a high specific strength and are therefore increasingly used for light‐weight constructions in transportation industry.[1,2] To predict…”
    Get full text
    Journal Article
  7. 7

    Microstructures and mechanical properties of pure Mg processed by rotary swaging by Gan, W.M., Huang, Y.D., Wang, R., Wang, G.F., Srinivasan, A., Brokmeier, H.-G., Schell, N., Kainer, K.U., Hort, N.

    Published in Materials in engineering (01-11-2014)
    “…•Grain size of pure Mg can be effectively reduced by rotary swaging processing.•The dominated texture of the swaged pure Mg was a basal fibre.•Twinning and…”
    Get full text
    Journal Article
  8. 8

    Deformation and texture evolution in AZ31 magnesium alloy during uniaxial loading by Yi, S.-B., Davies, C.H.J., Brokmeier, H.-G., Bolmaro, R.E., Kainer, K.U., Homeyer, J.

    Published in Acta materialia (2006)
    “…The anisotropic mechanical behavior of extruded AZ31 magnesium alloy is described in relation to the crystallographic texture. Specimens taken at 0°, 45° and…”
    Get full text
    Journal Article
  9. 9

    Effects of organic acid pickling on the corrosion resistance of magnesium alloy AZ31 sheet by Nwaogu, U.C., Blawert, C., Scharnagl, N., Dietzel, W., Kainer, K.U.

    Published in Corrosion science (01-06-2010)
    “…Organic acids were used to clean AZ31 magnesium alloy sheet and the effect of the cleaning processes on the surface condition and corrosion performance of the…”
    Get full text
    Journal Article
  10. 10

    Corrosion behavior of Mg–Gd–Zn based alloys in aqueous NaCl solution by Srinivasan, A., Blawert, C., Huang, Y., Mendis, C.L., Kainer, K.U., Hort, N.

    Published in Journal of magnesium and alloys (01-09-2014)
    “…The corrosion behavior of Mg-10Gd–xZn (x = 2, 6 wt.%) alloys in 0.5 wt.% NaCl solution was investigated. Microstructures of both the alloys consisted of…”
    Get full text
    Journal Article
  11. 11

    Evaluation of the delayed hydride cracking mechanism for transgranular stress corrosion cracking of magnesium alloys by Winzer, N., Atrens, A., Dietzel, W., Song, G., Kainer, K.U.

    “…This paper evaluates the important elements of delayed hydride cracking (DHC) for transgranular stress corrosion cracking (TGSCC) of Mg alloys. A DHC model was…”
    Get full text
    Journal Article
  12. 12

    Polycrystalline and amorphous MgZnCa thin films by Schlüter, K., Zamponi, C., Hort, N., Kainer, K.U., Quandt, E.

    Published in Corrosion science (01-10-2012)
    “…► Huge influence of deposition parameters on thin films’ microstructure. ► Significantly reduced corrosion rates for thin films with amorphous microstructure…”
    Get full text
    Journal Article
  13. 13

    In situ synchrotron diffraction of the solidification of Mg4Y3Nd by Tolnai, D., Mendis, C.L., Stark, A., Szakács, G., Wiese, B., Kainer, K.U., Hort, N.

    Published in Materials letters (01-07-2013)
    “…In situ synchrotron diffraction experiments were performed during the solidification of a Mg4Y3Nd alloy. The material was melted and solidified inside a sealed…”
    Get full text
    Journal Article
  14. 14

    Phase equilibria, thermodynamics and solidification microstructures of Mg–Sn–Ca alloys, Part 2: Prediction of phase formation in Mg-rich Mg–Sn–Ca cast alloys by Kozlov, A., Ohno, M., Leil, T. Abu, Hort, N., Kainer, K.U., Schmid-Fetzer, R.

    Published in Intermetallics (01-02-2008)
    “…The basis of this work is a detailed investigation of phase equilibria of the Mg–Sn–Ca system for wide ranges of composition and temperature by means of a…”
    Get full text
    Journal Article
  15. 15

    Fractography of Stress Corrosion Cracking of Mg-Al Alloys by Winzer, Nicholas, Atrens, A., Dietzel, W., Song, G., Kainer, K.U.

    “…Mechanisms for the stress corrosion cracking (SCC) of Mg-Al alloys have been investigated by scanning electron microscopy (SEM) of the fracture surfaces, for…”
    Get full text
    Journal Article
  16. 16

    Hydrostatic extrusion of commercial magnesium alloys at 100 °C and its influence on grain refinement and mechanical properties by Swiostek, J., Göken, J., Letzig, D., Kainer, K.U.

    “…Magnesium wrought alloys are of special interest for structural parts due to the possibility to obtain improved and more homogenous microstructures and…”
    Get full text
    Journal Article
  17. 17
  18. 18

    Creep behavior of AE42 based hybrid composites by Arunachaleswaran, A., Pereira, I.M., Dieringa, H., Huang, Y., Hort, N., Dhindaw, B.K., Kainer, K.U.

    “…Magnesium alloy based hybrid composites with varying levels of δ-alumina short fibers (Saffil f ®) and SiC particles (SiC p) reinforcements have been prepared…”
    Get full text
    Journal Article
  19. 19

    Thermal behavior of short fiber reinforced AlSi12CuMgNi piston alloys by Huang, Y.D., Hort, N., Kainer, K.U.

    “…The mismatch in thermal expansion coefficients could introduce large thermal stresses during thermal processing and correspondingly increase the dislocation…”
    Get full text
    Journal Article
  20. 20

    Orientation effects on acoustic emission during tensile deformation of hot rolled magnesium alloy AZ31 by Bohlen, J., Chmelı́k, F., Dobroň, P., Kaiser, F., Letzig, D., Lukáč, P., Kainer, K.U.

    Published in Journal of alloys and compounds (22-09-2004)
    “…Acoustic emission (AE) is observed during tensile testing of commercial AZ31 magnesium sheets in different temper conditions. Tests were conducted in rolling…”
    Get full text