Search Results - "Bokria, Jayesh G."
-
1
Poly(thieno[3,4-b]furan), a New Low Band Gap Polymer: Experiment and Theory
Published in Macromolecules (14-10-2008)“…A new optically transparent, near-infrared-absorbing low energy gap conjugated polymer, poly(thieno[3,4-b]furan) (PT34bF), with promising attributes for…”
Get full text
Journal Article -
2
Spatial effects in the photodegradation of poly(acrylonitrile-butadiene-styrene): a study by ATR-FTIR
Published in Polymer (Guilford) (01-05-2002)“…Spatial effects in the degradation of polyacrylonitrile-butadiene-styrene (ABS) exposed to ultraviolet radiation and oxygen in a weathering chamber at 318K…”
Get full text
Journal Article -
3
Degradation in photovoltaic encapsulant transmittance: Results of the first PVQAT TG5 artificial weathering study
Published in Progress in photovoltaics (01-05-2019)“…Reduced optical transmittance of encapsulants resulting from ultraviolet (UV) degradation is frequently identified as a cause of decreased performance through…”
Get full text
Journal Article -
4
Degradation in photovoltaic encapsulation strength of attachment: Results of the first PVQAT TG5 artificial weathering study
Published in Progress in photovoltaics (01-07-2020)“…Delamination of the encapsulant in photovoltaic (PV) module technology results in immediate optical loss and may enable subsequent corrosion or mechanical…”
Get full text
Journal Article -
5
Solid-State Conversion of Processable 3,4-Ethylenedioxythiophene (EDOT) Containing Poly(arylsilane) Precursors to π-Conjugated Conducting Polymers
Published in Advanced materials (Weinheim) (18-03-2008)“…The thermal degradation products of poly(methyl meth acrylate) model compounds in an ambient atmosphere were mapped via high‐resolution electrospray ionization…”
Get full text
Journal Article -
6
Variable-color poly(3,4-propylenedioxythiophene) electrochromics from precursor polymers
Published in Polymer (Guilford) (21-01-2010)“…We have developed two approaches to processable precursors to conjugated polymers: main-chain and side-chain. Upon oxidative conversion to the conjugated…”
Get full text
Journal Article -
7
Thermal Aging of Heterophasic Propylene−Ethylene Copolymers: Spatial and Temporal Aspects of Degradation Based on ESR, ESR Imaging, and FTIR
Published in Macromolecules (25-03-2003)“…Heterophasic propylene−ethylene copolymers (HPEC) containing bis(2,2,6,6-tetramethyl-4-piperidinyl) sebacate (Tinuvin 770) as a hindered amine stabilizer (HAS)…”
Get full text
Journal Article -
8
Thermal Aging of Heterophasic Propylene−Ethylene Copolymers: Morphological Aspects Based on ESR, FTIR, and DSC
Published in Macromolecules (25-03-2003)“…Electron spin resonance (ESR) spectra of nitroxide radicals formed in thermally treated heterophasic propylene−ethylene copolymers (HPEC) containing…”
Get full text
Journal Article -
9
Self-Assembling in Nafion Perfluorinated Ionomers Based on ESR Spectra of Novel Fluorinated Nitroxide Spin Probes
Published in The journal of physical chemistry. B (16-10-2003)“…ESR spectra of three fluorinated nitroxide radicals with different lengths of the fluorinated side chain were measured in neat solvents and in aqueous Nafion…”
Get full text
Journal Article -
10
Degradation in PV encapsulation transmittance: An interlaboratory study towards a climate-specific test
Published in 2015 IEEE 42nd Photovoltaic Specialist Conference (PVSC) (01-06-2015)“…Reduced optical transmittance of encapsulants resulting from ultraviolet (UV) degradation has frequently been identified as a cause of decreased PV module…”
Get full text
Conference Proceeding -
11
Degradation in photovoltaic encapsulation strength of attachment: Results of the first PVQAT TG5 artificial weathering study
Published in Progress in photovoltaics (12-03-2020)“…Delamination of the encapsulant in photovoltaic (PV) module technology results in immediate optical loss and may enable subsequent corrosion or mechanical…”
Get full text
Journal Article -
12
Degradation in PV encapsulant strength of attachment: An interlaboratory study towards a climate-specific test
Published in 2016 IEEE 43rd Photovoltaic Specialists Conference (PVSC) (01-06-2016)“…Reduced strength of attachment of the encapsulant resulting from the outdoor environment, including ultraviolet (UV) radiation, may decrease photovoltaic (PV)…”
Get full text
Conference Proceeding