Search Results - "Andersson, J.M."

Refine Results
  1. 1

    Scratch adhesion characteristics of PVD TiAlN deposited on high speed steel, cemented carbide and PCBN substrates by Sveen, S., Andersson, J.M., M’Saoubi, R., Olsson, M.

    Published in Wear (30-11-2013)
    “…Modern tool materials, ranging from powder metallurgical high speed steel to super hard materials such as polycrystalline cubic boron nitride and diamond, are…”
    Get full text
    Journal Article
  2. 2

    Enhanced thermal stability and fracture toughness of TiAlN coatings by Cr, Nb and V-alloying by Chen, Y.H., Roa, J.J., Yu, C.H., Johansson-Jõesaar, M.P., Andersson, J.M., Anglada, M.J., Odén, M., Rogström, L.

    Published in Surface & coatings technology (25-05-2018)
    “…The effect of metal alloying on mechanical properties including hardness and fracture toughness were investigated in three alloys, Ti~0.33Al0.50(Me)~0.17N…”
    Get full text
    Journal Article Publication
  3. 3

    Structural effects of energy input during growth of Ti1−xAlxN (0.55≤x≤0.66) coatings by cathodic arc evaporation by Andersson, J.M., Vetter, J., Müller, J., Sjölén, J.

    Published in Surface & coatings technology (01-02-2014)
    “…Effects of growth conditions on structural properties are investigated for the case of Ti1−xAlxN (0.55≤x≤0.66) deposition by cathodic arc evaporation. The…”
    Get full text
    Journal Article
  4. 4
  5. 5

    Phase tailoring of Ta thin films by highly ionized pulsed magnetron sputtering by Alami, J., Eklund, P., Andersson, J.M., Lattemann, M., Wallin, E., Bohlmark, J., Persson, P., Helmersson, U.

    Published in Thin solid films (26-02-2007)
    “…Ta thin films were grown on Si substrates at different inclination angles with respect to the sputter source using high power impulse magnetron sputtering…”
    Get full text
    Journal Article
  6. 6

    Phase control of Al2O3 thin films grown at low temperatures by ANDERSSON, J. M, WALLIN, E, HELMERSSON, U, KREISSIG, U, MÜNGER, E. P

    Published in Thin solid films (14-08-2006)
    “…Low-temperature growth (500 deg C) of D*a-Al2O3 thin films by reactive magnetron sputtering was achieved for the first time. The films were grown onto Cr2O3…”
    Get full text
    Journal Article
  7. 7
  8. 8

    Mechanical integrity of PVD TiAlN-coated PcBN: Influence of substrate bias voltage and microstructural assemblage by Gordon, S., Rodriguez-Suarez, T., Roa, J.J., M'Saoubi, R., Andersson, J.M., Jiménez-Piqué, E., Llanes, L.

    Published in Ceramics international (15-02-2024)
    “…Polycrystalline cubic boron nitrides (PcBN) have been increasingly used together with PVD coatings, mainly for hard turning operations. Within this context,…”
    Get full text
    Journal Article
  9. 9

    Strain and phase evolution in TiAlN coatings during high-speed metal cutting: An in operando high-energy x-ray diffraction study by Moreno, M., Andersson, J.M., Eriksson, J., Alm, P., Hedström, K., M'Saoubi, R., Schramm, I.C., Schell, N., Johansson-Jöesaar, M.P., Odén, M., Rogström, L.

    Published in Acta materialia (2024)
    “…We report on phase and strain changes in Ti 1-x Al x N (0 ≤ x ≤ 0.61) coatings on cutting tools during turning recorded in operando by high-energy x-ray…”
    Get full text
    Journal Article
  10. 10

    Structural changes in Ti1-xAlxN coatings during turning: A XANES and EXAFS study of worn tools by Rogström, L., Moreno, M., Andersson, J.M., Johansson-Jöesaar, M.P., Odén, M., Klementiev, K., Näslund, L.-Å., Magnuson, M.

    Published in Applied surface science (01-03-2023)
    “…[Display omitted] •Phase changes in worn TiAlN coated tools were studied by XANES and EXAFS.•Ti 1s XANES line-scans across the tool-chip contact were…”
    Get full text
    Journal Article
  11. 11

    Microstructure and wear mechanisms of texture-controlled CVD α-Al2O3 coatings by M’Saoubi, R., Alm, O., Andersson, J.M., Engström, H., Larsson, T., Johansson-Jõesaar, M.P., Schwind, M.

    Published in Wear (15-04-2017)
    “…In the present study, the microstructure and wear mechanisms of texture controlled CVD α-Al2O3 layers with (001), (012) and (100) growth textures were…”
    Get full text
    Journal Article
  12. 12

    The effect of nitrogen vacancies on initial wear in arc deposited (Ti0.52,Al0.48)Ny, (y < 1) coatings during machining by Calamba, K.M., Johansson Jõesaar, M.P., Bruyère, S., Pierson, J.F., Boyd, R., Andersson, J.M., Odén, M.

    Published in Surface & coatings technology (25-01-2019)
    “…Nitrogen deficient c-(Ti0.52Al0.48)Ny, y = 0.92, y = 0.87, and y = 0.75 coatings were prepared in different N2/Ar discharges on WC-Co inserts by reactive…”
    Get full text
    Journal Article
  13. 13

    Wear mechanisms of PVD-coated PCBN cutting tools by M’Saoubi, R., Johansson, M.P., Andersson, J.M.

    Published in Wear (01-04-2013)
    “…The wear characteristics of PVD coated (TiN, TiSiN, TiAlN, and AlCrN) polycrystalline cubic boron nitride (PCBN) cutting tools were compared to those of…”
    Get full text
    Journal Article Conference Proceeding
  14. 14

    Exploring the high entropy alloy concept in (AlTiVNbCr)N by Yalamanchili, K., Wang, F., Schramm, I.C., Andersson, J.M., Johansson Jöesaar, M.P., Tasnádi, F., Mücklich, F., Ghafoor, N., Odén, M.

    Published in Thin solid films (31-08-2017)
    “…We have explored the high entropy alloy (HEA) concept in the AlTiVNbCr-nitride material system. (AlTiVNbCr)N coatings synthesized by reactive cathodic arc…”
    Get full text
    Journal Article
  15. 15

    Growth of hard amorphous TiAlSiN thin films by cathodic arc evaporation by Fager, H., Andersson, J.M., Lu, J., Jöesaar, M.P. Johansson, Odén, M., Hultman, L.

    Published in Surface & coatings technology (25-11-2013)
    “…Ti1−x−yAlxSiyNz (0.02≤x≤0.46, 0.02≤y≤0.28, and 1.08≤z≤1.29) thin films were grown on cemented carbide substrates in an industrial scale cathodic arc…”
    Get full text
    Journal Article
  16. 16
  17. 17

    Pressurised hot water extraction with on-line particle formation by supercritical fluid technology by Andersson, J.M., Lindahl, S., Turner, C., Rodriguez-Meizoso, I.

    Published in Food chemistry (15-10-2012)
    “…► Pressurised hot water extraction is combined with supercritical carbon dioxide to dry extracts. ► The WEPO process stands for water extraction and particle…”
    Get full text
    Journal Article
  18. 18

    Effect of silicon content on PVD film mechanical properties and cutting performance of coated cemented carbide inserts by Bouzakis, K.-D., Bouzakis, E., Kombogiannis, S., Paraskevopoulou, R., Skordaris, G., Makrimallakis, S., Katirtzoglou, G., Pappa, M., Gerardis, S., M’Saoubi, R., Andersson, J.M.

    Published in Surface & coatings technology (25-12-2013)
    “…The paper investigates the effect of Si content on TiAlSiN, TiSiN and TiAlN/TiSiN films mechanical strength, brittleness, fatigue and adhesion. The films used…”
    Get full text
    Journal Article Conference Proceeding
  19. 19

    Influence of residual water on magnetron sputter deposited crystalline Al 2O 3 thin films by Wallin, E., Andersson, J.M., Lattemann, M., Helmersson, U.

    Published in Thin solid films (2008)
    “…The effects of residual water on the phase formation, composition, and microstructure evolution of magnetron sputter deposited crystalline alumina thin films…”
    Get full text
    Journal Article
  20. 20

    Phase control of Al 2O 3 thin films grown at low temperatures by Andersson, J.M., Wallin, E., Helmersson, U., Kreissig, U., Münger, E.P.

    Published in Thin solid films (2006)
    “…Low-temperature growth (500 °C) of α-Al 2O 3 thin films by reactive magnetron sputtering was achieved for the first time. The films were grown onto Cr 2O 3…”
    Get full text
    Journal Article