Search Results - "Agüero, Alina"

Refine Results
  1. 1

    Quasicrystalline Coatings Exhibit Durable Low Interfacial Toughness with Ice by Mohseni, Majid, Recla, Letícia, Mora, Julio, Gallego, Paloma García, Agüero, Alina, Golovin, Kevin

    Published in ACS applied materials & interfaces (04-08-2021)
    “…Ice accretion can adversely impact many engineering structures in commercial and residential sectors. Although there are many reports of…”
    Get full text
    Journal Article
  2. 2

    Three-dimensional imaging and characterization of the oxide scale formed on a polycrystalline nickel-based superalloy by Lech, Sebastian, Kruk, Adam, Gil, Aleksander, Cempura, Grzegorz, Agüero, Alina, Czyrska-Filemonowicz, Aleksandra

    Published in Scripta materialia (01-07-2019)
    “…Oxide scale formed on a polycrystalline nickel-based superalloy was investigated using analytical electron microscopy combined with three-dimensional…”
    Get full text
    Journal Article
  3. 3

    Microstructural studies of the scale on Sanicro 25 after 25,000 h of oxidation in steam using advanced electron microscopy techniques by Cempura, Grzegorz, Gil, Aleksander, Agüero, Alina, Gutiérrez, Marcos, Kruk, Adam, Czyrska-Filemonowicz, Aleksandra

    Published in Surface & coatings technology (15-11-2019)
    “…In the present study the effect of long-term oxidation at 700 °C in steam on the microstructure of Sanicro 25® (42Fe22Cr25NiWCuNbN) was investigated in detail…”
    Get full text
    Journal Article
  4. 4

    Three-dimensional characterization of an oxide scale on ATI 718Plus® superalloy by Kruk, Adam, Lech, Sebastian, Gil, Aleksander, Cempura, Grzegorz, Agüero, Alina, Wusatowska-Sarnek, Agnieszka M., Czyrska-Filemonowicz, Aleksandra

    Published in Corrosion science (01-06-2020)
    “…•FIB-SEM tomography supported by advanced TEM was an effective tool for 3D characterization of phases in oxidized 718Plus.•A discontinuous δ-Ni3Nb phase…”
    Get full text
    Journal Article
  5. 5

    Thermal cyclic resistance and long term inter-diffusion properties of slurry aluminide coatings modified with Si by Agüero, Alina, Landeira Østergård, María José, Hansson, Anette N., Gutierrez, Marcos

    Published in Results in surfaces and interfaces (01-02-2022)
    “…High temperature oxidation resistant aluminide coatings fail due to their inability to maintain a protective scale. The corresponding mechanism of protection…”
    Get full text
    Journal Article
  6. 6
  7. 7

    Microstructures of thin and thick slurry aluminide coatings on Inconel 690 by Rasmussen, Anders Juul, Agüero, Alina, Gutierrez, Marcos, José Landeira Østergård, María

    Published in Surface & coatings technology (15-01-2008)
    “…Two slurry aluminide coatings are produced on the Ni-base super alloy Inconel 690 by applying two different thicknesses of the same slurry on to the 690…”
    Get full text
    Journal Article
  8. 8

    Rapid α‑Al2O3 Growth on an Iron Aluminide Coating at 600 °C in the Presence of O2, H2O, and KCl by Agüero, Alina, Audigié, Pauline, Rodríguez, Sergio, Gutiérrez del Olmo, Marcos, Pascual, Jon, Ssenteza, Vicent, Jonsson, Torbjörn, Johansson, Lars-Gunnar

    Published in ACS applied materials & interfaces (30-10-2024)
    “…In this work, a slurry iron aluminide-coated ferritic steel SVM12 was subjected to a laboratory experiment mimicking superheater corrosion in a biomass-fired…”
    Get full text
    Journal Article
  9. 9

    Multiscale Characterization of an Oxide Scale Formed on the Creep-Resistant ATI 718Plus Superalloy during High-Temperature Oxidation by Kruk, Adam, Gil, Aleksander, Lech, Sebastian, Cempura, Grzegorz, Agüero, Alina, Czyrska-Filemonowicz, Aleksandra

    Published in Materials (23-10-2021)
    “…The ATI 718Plus® is a creep-resistant nickel-based superalloy exhibiting high strength and excellent oxidation resistance in high temperatures. The present…”
    Get full text
    Journal Article
  10. 10

    Accelerated aging of absorber coatings for CSP receivers under real high solar flux – Evolution of their optical properties by Reoyo-Prats, Reine, Carling Plaza, Alex, Faugeroux, Olivier, Claudet, Bernard, Soum-Glaude, Audrey, Hildebrandt, Christina, Binyamin, Yaniv, Agüero, Alina, Meißner, Tobias

    Published in Solar energy materials and solar cells (01-05-2019)
    “…The use of durable high solar absorptance receivers is a key element in a CSP plant project. In this article, different receiver materials are studied: four…”
    Get full text
    Journal Article
  11. 11

    Dynamic corrosion testing of metals in solar salt for concentrated solar power by Sutter, Florian, Oskay, Ceyhun, Galetz, Mathias Christian, Diamantino, Teresa, Pedrosa, Fátima, Figueira, Isabel, Glumm, Stefan, Bonk, Alexander, Agüero, Alina, Rodríguez, Sergio, Reche-Navarro, Tomás Jesus, Caron, Simon

    Published in Solar energy materials and solar cells (01-10-2021)
    “…Potassium nitrate and sodium nitrate in mixing proportion of KNO3–NaNO340-60 wt% (also called solar salt) has been successfully used for over a decade as heat…”
    Get full text
    Journal Article
  12. 12

    Robust anti-icing superhydrophobic aluminum alloy surfaces by grafting fluorocarbon molecular chains by Rico, Víctor, Mora, Julio, García, Paloma, Agüero, Alina, Borrás, Ana, González-Elipe, Agustín R., López-Santos, Carmen

    Published in Applied materials today (01-12-2020)
    “…•Robust anti-icing superhydrophobic alloy surfaces by grafting fluorocarbon molecular chains.•anti-icing textured aluminum surface by grafted fluorocarbon…”
    Get full text
    Journal Article
  13. 13
  14. 14

    Comparison of descaling methods to study the corrosion kinetics of ferritic steels after dynamic exposure to molten carbonates by Audigié, Pauline, Rodríguez, Sergio, Agüero, Alina, Pedrosa, Fatima, Paiva, Teresa, Diamantino, Teresa C.

    Published in Corrosion science (01-12-2022)
    “…T91 ferritic-martensitic steel was exposed to Li, Na and K molten carbonates at 650ºC under dynamic conditions up to 1000 h. After testing, three descaling…”
    Get full text
    Journal Article
  15. 15
  16. 16

    Long exposure steam oxidation testing and mechanical properties of slurry aluminide coatings for steam turbine components by Agüero, Alina, Muelas, Raúl, Pastor, Ana, Osgerby, Steve

    Published in Surface & coatings technology (21-11-2005)
    “…Important efforts to develop new steels or to protect high creep strength steels in order to allow operation of steam turbines at 650 °C are being carried out…”
    Get full text
    Journal Article Conference Proceeding
  17. 17

    Rapid α-Al 2 O 3 Growth on an Iron Aluminide Coating at 600 °C in the Presence of O 2 , H 2 O, and KCl by Agüero, Alina, Audigié, Pauline, Rodríguez, Sergio, Gutiérrez Del Olmo, Marcos, Pascual, Jon, Ssenteza, Vicent, Jonsson, Torbjörn, Johansson, Lars-Gunnar

    Published in ACS applied materials & interfaces (30-10-2024)
    “…In this work, a slurry iron aluminide-coated ferritic steel SVM12 was subjected to a laboratory experiment mimicking superheater corrosion in a biomass-fired…”
    Get full text
    Journal Article
  18. 18

    Oxidation under pure steam: Cr based protective oxides and coatings by Agüero, Alina, González, Vanessa, Gutiérrez, Marcos, Muelas, Raúl

    Published in Surface & coatings technology (25-12-2013)
    “…At temperatures of 900°C and higher, the formation, transformation and failure of protective oxides in air have been deeply studied. However, there is…”
    Get full text
    Journal Article Conference Proceeding
  19. 19

    Microstructure of an oxide scale formed on ATI 718Plus superalloy during oxidation at 850 °C characterised using analytical electron microscopy by Lech, Sebastian, Gil, Aleksander, Cempura, Grzegorz, Agüero, Alina, Kruk, Adam, Czyrska-Filemonowicz, Aleksandra

    “…The microstructure of a scale formed on the ATI 718Plus superalloy during oxidation at 850 °C for up to 1 000 h in air was characterised using various electron…”
    Get full text
    Journal Article Trade Publication Article
  20. 20

    Anomalous steam oxidation behavior of a creep resistant martensitic 9 wt. % Cr steel by Agüero, Alina, González, Vanessa, Mayr, Peter, Spiradek-Hahn, Krystina

    Published in Materials chemistry and physics (15-08-2013)
    “…The efficiency of thermal power plants is currently limited by the long-term creep strength and the steam oxidation resistance of the commercially available…”
    Get full text
    Journal Article